[MW:29006] Tube to tube sheet qualification

Dear sir,

I want know about Qualification of tube to tube sheet .
Test piece size
No of test
And clause

Regards,

Rohan soni
8238850741

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

1 comment:

SHOAIB said...

SEE AMSE SEC IX QW 193