Thursday, January 17, 2019

Re: [MW:28925] Re: Acceptance criteria for tensile test for WPS qualification

Yes, if your tensile is already achieved minimum UTS in what it required then it is accepted, as you are saying fracture in weld metal, i would like to know patterns of initiation.

FYI
https://www.twi-global.com/technical-knowledge/job-knowledge/mechanical-testing-tensile-testing-part-2-070


Regards,
Mohamed Muneeb Mahaboob
CSWIP 3.2-89247/2 
IRCA-9001:2015 LA
ASNT-NDT-L2-RTFI-RT-UT-MT-PT.
SAP#:70021650 APs:JAPID, QCS & QCI.
muneebslsa@gmail.com +91-636-955-7189
''If you know any art by any means then SCULPT IT - no matter how cheap or useless it is - JUST SCULPT ITyou will never know when experts will be on demand'' 
 
Date: 2019-01-16 21:43
Subject: [MW:28920] Re: Acceptance criteria for tensile test for WPS qualification
so what is problem, u got tensile strength more than the minimum tensile strength of base metal asme sec 9. its mean ur joint tensle strength is more than the base metal its ok .

On Tuesday, 15 January 2019 20:47:37 UTC+5:30, Megnath wrote:

Dear Experts,

Kindly share, if there is any code case interpretations or similar explanation in any of the international codes for the following issue.

Acceptance criteria for tensile test for WPS qualification.

If the specimen fails at weld metal (for ex. Exactly at weld centre) with higher tensile strength than base metal, what is the interpretation?

Thanks & Regards,
Megnath
Cochin

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...