Dear Sir,
I want to do WPS for Astm A128 Grade B1 tto astm a128 grade B1.
Which electrode to be follow
Raghavan QC
On Thu 24 Jan, 2019, 07:47 Pravin Poornachandran <htcispravin@gmail.com wrote:
Dear Expert,Good morning.Seeking for your expertise in suitable welding consumable for below material:SS904 to SS904LCS A105 to SS904LKindly advice.PravinSingapore--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
Comments