Dear
Obviously the valve closer test is the seat tight test only.
On Thu, Jan 31, 2019, 4:21 PM Raghuram Bathula <raghurambathula@gmail.com wrote:
--any member such as a ball, clapper, disc, gate, or plug, that is positioned in the flow stream to permit or preventflow. refer API598On Thu, 31 Jan 2019 at 14:45, chiluka venkatramulu <ramuluchiluka@gmail.com> wrote:Dear All,,Is the Valve closer test means sheet leak test or body pneumatic test?Venkatramulu
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
Comments