Re: [MW:28997] Using API 5LX65 FLG instead of A350 LF2 during qualification of A333 GR 6 P1G1 to P1G2

You dont need to use a flange for the PQR. Just pick a pipe material with same P no, and if impact testing is required with same Group No.
Keep in mind that in asme diameter is not an essential variable for PQR. 
Make your life easier by using large diameter samples 

Στις Παρ, 26 Οκτ 2018, 09:12 ο χρήστης Noor Osama <noorkathir@gmail.com> έγραψε:
Dear Expert,

Is it possible to replace LTCS Flange A350 LF2 by Flange API 5L X65 during qualification of A333 GR 6 Pipes to A350 LF2 Flange.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...