Re: [MW:28931] Bolt torquing values

Greetings,

Refer ASME PCC-1 for Bolt torque values.

Regards,
Sajeev

On Wed 16 Jan, 2019, 17:47 Hisham Al-Metwally <eng.hisham19@gmail.com wrote:
Hi all,
Where is it mentioned the torque values for bolts A193 for flange connections ?!

Thanks and regards
Hisham Almetwally
QC Engineer & Welding Engineer
Mob: +971564337326 & +971526679935

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...