special electrode available to avoid purging
THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE, CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer.
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349
--Even you can try with SS pipe root with SMAW without back purging.Thanks.
Regards,Mohamed Muneeb MahaboobCSWIP 3.2-89247/2IRCA-9001:2015 LAASNT-NDT-L2-RTFI-RT-UT-MT-PT.SAP#:70021650 APs:JAPID, QCS & QCI.''If you know any art by any means then SCULPT IT - no matter how cheap or useless it is - JUST SCULPT IT, you will never know when experts will be on demand''Dear Experts,--As per clause 7.3 of API RP 582 Ed. 2016 back purging required for GTAW & GMAW process but no where I could found for other process like SMAW. Is it mean that if we do welding with SMAW process back purging is not required?Please share your interpretation.Thanks and regardsManoj.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
Comments