Re: [MW:28143] Weld bead length

Greetings,

Debate regarding weaving starts with fact that many of WPS  states weaving as 3 times diameter, without any particular need. However, for 9 mm width, I believe no standard mandates multi-weave. At maximum, heat input can be measured and co related with pqr value.

Regards
AHS


On Thu, Jul 26, 2018 at 9:59 PM, Nadakuditi kiran kumar
<kinnu78@gmail.com> wrote:
Dear Gentlemen,
We are doing welding of LTCS materials, while welding some of the
joints we welded final run in single bead which is as per approved
WPS(3 x electrode dia.)  Our client is asking us to do multi bead
welding above 6" pipe even though the gap in groove is below 9 mm. We
are using 3.15 electrode to do the final run. We are maintaining heat
in put in control. Please clarify me whether it is correct or not?

Thanks & Regards

N.Kiran kumar,

--
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...