hiii
-- In PMI test by using x-ray fluorescence machine , it is very difficulty to get level of nitrogen ,carbon ,sulfer etc.I think you can find out this element by using optical emission spectograph machine.
Regards
Raneesh-QA/QC-Welding
UAE
On Monday, July 30, 2018 at 7:06:50 AM UTC+4, ken wrote:
On Monday, July 30, 2018 at 7:06:50 AM UTC+4, ken wrote:
SirsDuring weld metal Analysis of ER 90 S - B9 welded on P-91 material. According to ASME SEC II part C SFA 5.28 below table. 1 , Notes-: h/i/j applicable. How to measure Nitrogen by using PMI.Same time, is it mandatory to mention field PMI reports.Thanks & Regards
PRADEEPKUMAR HORMIS
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
Comments