Friday, July 27, 2018

Re: [MW:28139] Weld bead length

All,

Your client is right, multi bead welding  for cover pass - with SMAW - ensures fine grain weld metal and eliminates the risk of undercut which is the result of high amperage and incorrect electrode control.

regards,

Steve Burik, IWE



On ‎Thursday‎, ‎July‎ ‎26‎, ‎2018‎ ‎11‎:‎59‎:‎59‎ ‎AM, Nadakuditi kiran kumar <kinnu78@gmail.com> wrote:


Dear Gentlemen,
We are doing welding of LTCS materials, while welding some of the
joints we welded final run in single bead which is as per approved
WPS(3 x electrode dia.)  Our client is asking us to do multi bead
welding above 6" pipe even though the gap in groove is below 9 mm. We
are using 3.15 electrode to do the final run. We are maintaining heat
in put in control. Please clarify me whether it is correct or not?

Thanks & Regards

N.Kiran kumar,

--
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...