Tuesday, July 24, 2018

[MW:28128] NCR for leak found in water filling

Dear All

My client raised NCR for founding leakage during water fill on GRE pipe at run pipe. Leak found During time of water filling and  before starting hydro test.

Could any body please explain me raised NCR is acceptable or not.

AS per ITP- 6.3 is water filling stage
                    6.4 is hydro test.

Please reply me in urgent basis.


Regards
Srinivasan.A

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...