Sirs

During weld metal Analysis of ER 90 S - B9 welded on P-91 material. According to ASME SEC II part C  SFA 5.28 below table. 1 , Notes-: h/i/j applicable. How to measure Nitrogen by using PMI.
Same time, is it mandatory to mention field PMI reports.

Thanks & Regards

PRADEEPKUMAR HORMIS

Image result for QUALITY INSPECTION GIFS

 
 


 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...