Re: [MW:28114] CRITERIA OF CLAD THICKNESS

I Know that it must be 3 layers of weld metal deposition
Alcindo O. J. Jr.
21 98575-6362



Em seg, 23 de jul de 2018 às 11:24, Ali Asghari <asgharialigl@gmail.com> escreveu:
Dear All.

Does anybody know about how a designer calculate the thickness of clad material especially for sour service and how much is conservative?
because in our project documents have not said clearly that thickness of clad have to be measured from base material or from layer that dilution is negligible and this question remained does designer account or consider dilution or not?

Regards.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...