Dear Mr. Shaikh,
If the PQR is qualified with E7018, you can use E7018-1 but need to prepare a new WPS with E7018-1 provided meeting the requirements of all other essential & supplementary essential variables.
Refer attached file of asme code interpretation.
Regards,
Navnitkumar Parikh
On Tue, Jul 17, 2018 at 8:39 PM, Hasin Shaikh <hasin.shaikh@gmail.com> wrote:
Dear All--I have query about use of Electrode with change og classificationWe have WPS for SMAW welding process for P1 material with the E 7018 electrode in that case can we use in production E7018-1 electrodePlease help me out in interpretationQW 404.12 (e) from a classification that requires toughness testingto the same classification which has a suffix which indicatesthat toughness testing was performed at a lowertemperature or exhibited greater toughness at the requiredtemperature or both, as compared to the classificationwhich was used during procedure qualification (i.e., achange from E7018 to E7018‐1)
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com .
Visit this group at https://groups.google.com/group/materials-welding .
For more options, visit https://groups.google.com/d/optout .
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
Comments