[MW:28091] Thickness of weld metal qualified on two or more pipe as per ASME Sec ix for welders table QW-452.1 (b)

Greetings,
Dear professionals,
Need your opinions and experience on below case.
Welders qualification as per ASME sec. ix for thickness qualification, can we use different thickness pipes as per Table QW-452.1 (b) Note (2) Two or more pipe test coupons with different weld metal thickness may be used to determine the weld metal thickness qualified and that thickness may be applied to production welds to the smallest diameter for which the welder is qualified in accordance with Table QW-452.3
One welder with below thickness qualifications.
Test A:
GTAW 4mm & SMAW 7.08mm qualified.
Test B:
GTAW 4mm & SMAW 22.98 mm qualified.
His qualification for GTAW 8mm? and SMAW Unlimited as per above note 2?
Noted: for reference images are attached.
Waiting for your valuable comments with references.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...