Tuesday, July 24, 2018

Re: [MW:28114] USE OF ELECTRODE

Hi,

Write a new WPS with E7018-1 and sign off.

On Mon, Jul 23, 2018 at 10:54 AM, Hasin Shaikh <hasin.shaikh@gmail.com> wrote:
Dear Mr. Parikh

Thanks,as we have WPS without Impact test With E-7018,IN that case what should we do.


On Thu, Jul 19, 2018 at 11:32 AM, navnitkumar parikh <parikhnavnitkumar@gmail.com> wrote:
Dear Mr. Shaikh,

If the PQR is qualified with E7018, you can use E7018-1 but need to prepare a new WPS with E7018-1 provided meeting the requirements of all other essential & supplementary essential variables.

Refer attached file of asme code interpretation.

Regards,
Navnitkumar Parikh

On Tue, Jul 17, 2018 at 8:39 PM, Hasin Shaikh <hasin.shaikh@gmail.com> wrote:
Dear All

I have query about use of Electrode with change og classification 

We have WPS for SMAW welding process for P1 material with the E 7018 electrode in that case can we use in production E7018-1 electrode 

Please help me out in interpretation

QW 404.12 (e) from a classification that requires toughness testing
to the same classification which has a suffix which indicates
that toughness testing was performed at a lower
temperature or exhibited greater toughness at the required
temperature or both, as compared to the classification
which was used during procedure qualification (i.e., a
change from E7018 to E7018‐1)

--
*With Regards
Shaikh.Hasin
Email: hasin.shaikh@gmail.com
Mobile: +91-9924562942*


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.



--
*With Regards
Shaikh.Hasin
Email: hasin.shaikh@gmail.com
Mobile: +91-9924562942*


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.



--
Regards,
Nithin Joseph Dsilva
+971 557645785

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...