Monday, January 16, 2017

Re: [MW:25895] 308/308L electrode

All basic electrodes need to be conditioned in not delivered in sealed packs or not used



Sent from my Samsung Galaxy smartphone.

-------- Original message --------
From: Rupesh Sao <rupesh7231@gmail.com>
Date: 14/01/2017 09:58 (GMT+02:00)
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:25888] 308/308L electrode

Dear All,
As far i know and used to not to backing of SS electrode, but it is found that on manufactures cover it show to re-dry up to 150-200'c.
If it is required to back;
In which condition (Atmospherics)
In any special coated flux electrode
or
we need to back all kind of 308 electrodes????

Please suggest.

Thank you all
Rupesh Ssao

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/d1f3c1ad-e951-4f55-bd0d-43450c44e8a2%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...