Friday, January 27, 2017

Re: [MW:25993] PQR with E350

No, you need a new PQR

2017-01-27 11:48 GMT+02:00 Vijay Katkar <katkar.vijay22@gmail.com>:
Dear Experts,

I have PQR with IS 2062 E350BR which is not given in ASME Section IX and I have consider this as unassigned material.
I want to use this PQR for welding of E250 material which given in ASME section IX as P No 1 & Gr No 1.

As far as my knowledge we can not use this PQR for E250 welding.

Is their any clause can help me to use E350BR PQR for E250 material welding?

Thanks

Vijay Katkar

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAP37wrK23Eo9N44H28LTQi2bZ%3DBqHvkoPYo%3DuwPWikrQ4VU-vA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40DO2_TKjd8ar-6_au9ydpBv1FDWQUPHDM4hMZZ3bitDWQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.