RE: [MW:25936] Sec. IX- QW-403.5

If impact qualification is not required;  Yes.

 

If impact qualification is required:  No

 

See QG-105.3 and QW-200.1(b)

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Unni Romes
Sent: Wednesday, January 18, 2017 5:41 AM
To: Materials & Welding
Subject: [MW:25924] Sec. IX- QW-403.5

 

Dear all,

 

Please be clarified, 

 

SMAW, PQR is qualified with P1, G1 to P1, G1, 

 

as group number is supplimentary, 

 

Does this PQR support the WPS for P1 G1 to P1 G2

 

Is there any interpretation reference for this? 

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/a1a6fa46-8cc1-41c7-ade8-f0f0f5a8bc33%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...