Re: [MW:25996] Thin wall, small dia tube weld repair

Thanks, George.
The shop is certified for the job, but they do not know for sure how to access the defect area for its removal and re-welding.
Small size grinder with extendable arm, FCAW process...etc.
 
Best Regards,
Shashank C Vagal 
301, PRATHAMESH, M G Rd – Mahant Rd, Vile Parle East, Mumbai 400 057 INDIA
Tel : +91 22 2611 6640 / (+91) 9821386292 /  8082395502



From: George Dilintas <dilintas@gmail.com>
To: Meghanadh K <materials-welding@googlegroups.com>
Sent: Friday, 27 January 2017 6:15 PM
Subject: Re: [MW:25995] Thin wall, small dia tube weld repair

Check ASME PCC-2-2015

2017-01-26 15:33 GMT+02:00 'Shashank Vagal' via Materials & Welding <materials-welding@googlegroups.com>:
Dear all,
We have repairs in a weld at 180 mm from open end on 47 mm ID x 5 mm thick CS boiler tubes. The repairs are at various depths. Access is available only from ID, approach from OD is not possible. Is there any process by which defects can be removed / repaired. Suitable fixture for internal movement can be made available.
Please advise.
 
Best Regards,
Shashank C Vagal  
301, PRATHAMESH, M G Rd – Mahant Rd, Vile Parle East, Mumbai 400 057 INDIA
Tel : +91 22 2611 6640(+91) 9821386292 /  8082395502
--
http://www.linkedin.com/ groups/MaterialsWelding- 122787?home=&gid=122787&trk= anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@ googlegroups.com.
To post to this group, send email to materials-welding@ googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/ msgid/materials-welding/ 629460873.1291443. 1485437622847%40mail.yahoo.com .
For more options, visit https://groups.google.com/d/ optout.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40D8Txey8QN%3D_1hmPBYDSyVD3hTa%2BTTinbfEMFiLdxwYFw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.


No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...