We should not confuse between the WPS used for the PQR and a WPSS which will give direct instructions to welders on how to perform a specific weld.
Sent from my Samsung Galaxy smartphone.
-------- Original message --------
From: Unni Romes <unniromes@gmail.com>
Date: 18/01/2017 14:14 (GMT+02:00)
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:25924] Re: Socket Weld WPS
If the join design is not essential variable for that particular process and all the other essential variables are within the PQR range, the WPS for butt weld will be applicable for fillet and socket weld join designs which specified in the applicable code for fabrication and erection (ie, B31.1, B31.3 etc.)
On Tuesday, January 17, 2017 at 1:40:33 PM UTC+4, Ali Hayat wrote:
-- On Tuesday, January 17, 2017 at 1:40:33 PM UTC+4, Ali Hayat wrote:
Dear All,
Does butt weld WPS is applicable for socket weld? Can anyone provide ASME IX code reference for this ?
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/7aa0715e-d93e-4433-9787-393b78f2c5ec%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
Comments