Re: [MW:25918] Regarding 2% sensitivity in radiography film.

Check SE-1025 in  ASME V



Sent from my Samsung Galaxy smartphone.

-------- Original message --------
From: 'srinivasan muthukrishnan' via Materials & Welding <materials-welding@googlegroups.com>
Date: 16/01/2017 12:07 (GMT+02:00)
To: materials-welding@googlegroups.com, Prasad Rode <purode333@gmail.com>, Materials & Welding <materials-welding@googlegroups.com>
Subject: Re: [MW:25895] Regarding 2% sensitivity in radiography film.

For 1" RT technique suppose to be superimpose  technique(DWSI) ,so we need to calculate this way 

Double the thickness 4.1+4.1=8.2 and one reinforcement 1.5mm for 1" welding

0.20/9.7*100=2%


On Fri, 13 Jan, 2017 at 17:32, Prasad Rode
<purode333@gmail.com> wrote:
Dear sir,
Thanks for reply.

I want make clear my concept about sensitivity.
My point is that
1) sensitivity= thk of visible wire/ base metal thk * 100 ,
is it correct formula or not.

2) Secondly, according to client,  sensitivity means 2% of base metal. It will comes to 0.08mm for 4.1 mm thk base metal. Means, we have show IQI of 0.08mm.i.e. 1st wire of set A.

Request all experts, pls clear my concept about 2% sensitivity.

Regards
Prasad

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c460263c-22fc-4aad-add7-0d1a29879818%40googlegroups.com.

For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/561118560.4500874.1484561258016%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...