Re: [MW:25997] WELDER QUALIFICATION CERTIFICATE RENEWAL AS PER ASMESEC. IX

Make Welder log and welder continuity record for proof that the welder engagement for that qualified process. NDT proof not at  all required as per ASME Sec9, but it is required as per ISO 9606 for prolongation. As John said, if it is client requirement, Code is not applicable.


On 27-Jan-2017 7:54 PM, "George Dilintas" <dilintas@gmail.com> wrote:
Boxbe This message is eligible for Automatic Cleanup! (dilintas@gmail.com) Add cleanup rule | More info

NDT reports are not the only objective evidence.
Weld maps, welding logs could also provide objective evidence that no interruption using this process longer than 6 months occured

2017-01-25 9:28 GMT+02:00 Manoj John <manojacgnr@gmail.com>:
What evidence we can documented in such cases if there is no NDT.  Always everybody is looking for RT reports.

Thanks,

On Sun, Jan 22, 2017 at 9:11 PM, George Dilintas <dilintas@gmail.com> wrote:
The Code requires to have welded with the specific process within six months. No other requirement is set

2017-01-21 11:12 GMT+02:00 Manoj John <manojacgnr@gmail.com>:
Dear Friends,

We have qualified welders in groove welding (GTAW+SMAW) as per ASME section IX but they have welded 2 months butt welding and 4 months they welded only fillet joints. Now they completed 6 months and they are continuing welding.  

My question is how can we renew their certificates since they do not have any Radiography reports for fillet joints.  Can we renew their certificate with a visual inspection report.

Thanks & Regards.

Manoj John.


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACgUO5nBM2QU9Uv6y98y1YLy0gpA8sbUU88XHKG0LHHaeEnZ%3Dw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40DzKRAD6deB8b0iNCyYo00bymKj6ZcMNHgbUwwa420pHQ%40mail.gmail.com.

For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACgUO5nCPGOvvGb5dFDEribYwwPOfwku_k_N3sXAhwfjeqFBVQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40CViABarWDrxxzUrB8YSetXQjUG42GsDRp4OOkgUPpeKg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4ePcxQ_YfVixo8g9wnjEj5qxrhmNrWUsDE2s1afNrtN4nA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...