Because rolled plates have anisotropic properties.
Thinkba little bit on grains orientation and you will find out why



Sent from my Samsung Galaxy smartphone.

-------- Original message --------
From: ABHISHEK SINGH <mech.abhi17@gmail.com>
Date: 14/01/2017 09:59 (GMT+02:00)
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:25888] PQR plate transverse to rolling direction of plate

Dear Experts,
         Generally why it is preferred to cut PQR piece transverse to the rolling direction of plate.What is the technical reason behind this??

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/553dae23-e7b1-4100-874b-30038f99bf25%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...