Tuesday, January 17, 2017

[MW:25915] Combining 2 PQRS

Dear Expert,

I am having 2 PQRs i.e.:
1. 2" Sch. 80 Pipe (thk.-5.54mm) - GTAW (70S-2)
2. 6" Sch. 160 Pipe (thk.-18.26mm) - SMAW (7018)

My question is: Can I combine these 2 PQRs for buiding up one more making new WPS for 8" Sch. 80 Pipe (thk.-12.70mm) using GTAW+SMAW (Root and hot with GTAW and filling and capping with SMAW)

Thanx in advance

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c48bcc22-b50c-4d5a-8147-e4a0c3a3db39%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...