Re: [MW:25963] WELDER QUALIFICATION CERTIFICATE RENEWAL AS PER ASME SEC. IX

As per ASME IX, Renewal only for qualified Welding Process, with fillet weld u can 

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349

On Sat, Jan 21, 2017 at 2:42 PM, Manoj John <manojacgnr@gmail.com> wrote:
Boxbe This message is eligible for Automatic Cleanup! (manojacgnr@gmail.com) Add cleanup rule | More info

Dear Friends,

We have qualified welders in groove welding (GTAW+SMAW) as per ASME section IX but they have welded 2 months butt welding and 4 months they welded only fillet joints. Now they completed 6 months and they are continuing welding.  

My question is how can we renew their certificates since they do not have any Radiography reports for fillet joints.  Can we renew their certificate with a visual inspection report.

Thanks & Regards.

Manoj John.


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACgUO5nBM2QU9Uv6y98y1YLy0gpA8sbUU88XHKG0LHHaeEnZ%3Dw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eO2O_Qf68KQY%3DeYCJnSfq-HZ%3DdMg2j2HVTiNMC0gwzvrA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...