Dear Experts
We have one Vessel to fix baffle plates . Vessel is under service since 9 years. Shell thickness is 38 mm and baffles plates thickness will be 7mm. My question are:
1. Is R-stamp required or not? 2. Is local PWHT required or not?
Please share / send me answer with reference of codes
Thanks and Best Regards
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/EEE7D9CD-935A-43E5-8101-8668CA4B4A9C%40yahoo.com.
For more options, visit https://groups.google.com/d/optout.
Subscribe to:
Post Comments (Atom)
[MW:35748] Re: PQR- Chemical testing requirements
As answered by everyone, chemical is not required. Notwithstanding, please note that A-No. which denotes weld metal chemical composition is ...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-