Tuesday, May 31, 2016

Re: [MW:24917] Min BHN value

Try in B31.3. If not only in scientific publications relevant to creep resistance. For P91 the bibliography us giving 191HV minimum after PWHT

Sent from my BlackBerry 10 smartphone.
From: samaran sadasivam
Sent: Κυριακή, 29 Μαΐου 2016 - 13:32
To: materials-welding@googlegroups.com
Reply To: materials-welding@googlegroups.com
Subject: [MW:24902] Min BHN value

Dear Experts,

What is the minimum hardness value for alloy steel pipe material(A335 P11,P22,P5) and which code have to refer. Our contract documents specifies max. BHN value only. So, pls tell me the details.



Thanks & Regards
S.Samaran
+91 9486664977 

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGxS6aRdqrhfTSfhyzpvyTALt8X3oQT1JyksgBT9OaTw8h2R_g%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...