Tuesday, May 24, 2016

Re: [MW:24848] ISO 9606 (Welder Qualification)

NoBo is not required but Third party inspection or Manufacturer appointed person who is not reporting to Production

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349

On Mon, May 23, 2016 at 9:54 PM, <dilintas@gmail.com> wrote:
Neither in the PED nor in the guidelines a formal requirement for witnessing by NoBo.

Sent from my BlackBerry 10 smartphone.
From: Elsayed Elghareeb
Sent: Κυριακή, 8 Μαΐου 2016 - 12:57
Subject: Re: [MW:24773] ISO 9606 (Welder Qualification)

Acording to lSO 9606-1 point 6.1 it shall be done "yes"

On Sun, May 8, 2016 at 10:13 AM, Vijay Katkar <katkar.vijay22@gmail.com> wrote:

Do we need to appoint examinations body to quality each Welder as per ISO 9606?

On May 8, 2016 12:19 PM, "Prakash Gotimukul" <gprakash31@gmail.com> wrote:
Any notified body( NoBo) accredited to witness and certify welding procedures/welders

Rgds
Prakash Gotimukul
AIS, Consultant ASME/ISO/PEDlIBR
 Mob:+97152 979 5678

On Sat, May 7, 2016 at 8:02 PM, Vijay Katkar <katkar.vijay22@gmail.com> wrote:

Dear All,

Need your help on below topic.

What is the meaning of Examiner and examination body as per ISO 9606?

What is the criteria for Examiner ?

Can person from organization consider as Examiner?

Thank you

Vijay Katkar

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAP37wrKAVmiocWBfyBzJJFg0%3D2K7wHycFyySazUUmehq9NOQjQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOUP4q%2Byo7D5JOJA_A6_s7pZopHLxGY21tqRaKGcs7TXb%3DADJQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAP37wrJ03V6aUf%3DkkgVA2UN%2BFhneJZJQyVC81z0KJVnXMTSETQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.



--
Best Regardes,

 
Eng:- Elsayed Elghareeb.
Dipl. Welding Engineer.
DSD-FERROMETALCO.
+2 0100 82 61 645.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOCciGJiqeKuc30-4FzrA-6%3DERBnO3rCfUQ-N93qh3FY3U5S6A%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/20160523162423.6713426.14159.3074%40gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eOPSXm-YpjPEv8zV4g-kd0rpE2aadFPh-8bzUChdOuGmg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...