no problem with 308 in that case
2016-05-26 20:29 GMT+03:00 Mohd Siraj <mohd52100@gmail.com>:
what filler to be used for joining?--is 308L is okey?
On Tuesday, May 24, 2016 at 8:50:43 PM UTC-7, Makrand Sakpal wrote:Dears,
We have one atmospheric hygienic (Food Industry) vertical vessel of SS904L material which is supported on legs. Vessel diameter is 3200 mm & TL-TL is 5100 mm.
The question is, can we weld SS304 directly on SS904L so that we can use SA-312 TP304 pipe l;eg supports?
Is it necessary to have SS904L RF pad instead of SS304?
Can there be an issue with weldability of SS904L with SS304?
Note : - We can't go for skirt support option.
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/409451da-9d6f-4f95-9637-76f23c2fa9eb%40googlegroups.com.
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40CkKZY_R2odmB395NGXz8J_e6OioxdP%2Bj13gYCP5n36Ow%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Comments