Re: [MW:24910] IS 2062 safe working temperature

Hi

IS2062 Grade E410 B0 can be used upto zero degree celcius and max 300 degree celcius.
Quality C can be used to as low as minus 20 degree Celcius.

PREM S NAUTIYAL
CELL : 9769316004


From: Kadir godil <kadirgodil@gmail.com>
Sent: Mon, 30 May 2016 18:09:03
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:24908] IS 2062 safe working temperature
dear experts,

what is the safe working range of IS 2062 steel? 

please inform me about the standard where i can find this data?

thank you

sincerely,
kadir godil

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/b6c8669d-2e39-4058-a120-42eeba9651d2@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

Get your own FREE website, FREE domain & FREE mobile app with Company email.  
Know More >

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1464611943.S.7653.19149.f4-234-218.1464628317.30713%40webmail.rediffmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...