[MW:24885] Re: E6013 not Applicable for High Thickness material

moreover to Mr pandithan,

With E6010 slag removal is very easy.,

very thin slag of root will go away during piping hydrotest or flushing.

On Tuesday, May 24, 2016 at 4:19:59 AM UTC-7, Amit Vishwakarma wrote:
Dear Expert

It has been observed that practically that E6013 electrode generally used for low thickness material i.e less than 20mm thickness however E7018 become mandatory for high thickness on the same material in structural work.
Kindly give your opinion refer to standard.

Regards
Amit Vishwakarma

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/0ad33a46-564e-4a74-8af3-5bfbbc6f6b1c%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...