Wednesday, May 25, 2016

Re: [MW:24870] IQI selection.

IQI selection will be based on nominal single wall thickness plus estimated reinforcement only.
Refer ASME Sec V article 2.

PREM S NAUTIYAL
CELL : 9769316004


From: Prabir Kumar Singh <prabirkumarsingh86@gmail.com>
Sent: Wed, 25 May 2016 16:34:39
To: materials-welding <materials-welding@googlegroups.com>
Subject: [MW:24868] IQI selection.

What is effective thickness for IQI selection in DWSI and DWDI method. Sum of double wall thickness or only single wall thickness?

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOis+9vAHjU6WCt_zT1LgxzeYvQPhFwBsU-X4TeTOUy76Ujvcg@mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Get your own FREE website, FREE domain & FREE mobile app with Company email.  
Know More >

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1464174279.S.9600.32349.f4-235-104.1464192926.30654%40webmail.rediffmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...