[MW:24834] Re: Impact Test Acceptance Criteria for Dissimilar material PQR qualification

acceptable for subsize specimen

On Monday, 23 May 2016 17:12:18 UTC+4, Biplab Pal wrote:
Dear Gents,

Our Construction Code is ASME B 31.3.

Our Client standard is asking for the minimum impact value of 34/27 J for P1 Gr 1 & 40/32 J for P1 Gr 2 full size (10X10) specimens both Weld metal and HAZ at minimum design temperature for PQR qualification.

Process- GTAW + SMAW

Out MDMT is -45 Deg C.

The PQR tested at -64.7 deg C and the impact values are as follows for Weld 20.33/17 J and for HAZ-1 is 41.5/35.5 & HAZ-2 is 40/50 J.
Specimen size is 10X4.

Is the test result acceptable for Weld zone as per client std.?

We need your kind advice and code reference.


--
Thanks & Regards
Biplab Pal
Welding Inspector
E-mail:   biplab.mech@gmail.com
 

 

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/bc8d51c8-6bf4-4f67-b4d0-4a2398cb643f%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...