Hi!
You can weld by E308L consumables but you require to qualify PQR due to different P no
Regards
Hegde
On Thursday, 26 May 2016 10:59 PM, Mohd Siraj <mohd52100@gmail.com> wrote:
what filler to be used for joining?
-- is 308L is okey?
On Tuesday, May 24, 2016 at 8:50:43 PM UTC-7, Makrand Sakpal wrote:
On Tuesday, May 24, 2016 at 8:50:43 PM UTC-7, Makrand Sakpal wrote:
Dears,We have one atmospheric hygienic (Food Industry) vertical vessel of SS904L material which is supported on legs. Vessel diameter is 3200 mm & TL-TL is 5100 mm.The question is, can we weld SS304 directly on SS904L so that we can use SA-312 TP304 pipe l;eg supports?Is it necessary to have SS904L RF pad instead of SS304?Can there be an issue with weldability of SS904L with SS304?Note : - We can't go for skirt support option.
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/409451da-9d6f-4f95-9637-76f23c2fa9eb%40googlegroups.com.
Comments