As you stated , to combine 2 PQRs and generate a new WPS, your PQRs should be performed with material greater than 13mm.

2016-05-31 11:14 GMT+03:00 Demir Alp ILIKOBA <demiralp85@gmail.com>:

Dear Experts; 


  I would like to get your professional opinion on combination of PQRs as per ASME Section IX QW-200.4   I have 2 PQRs (w/back-gouging) and I would like to combine these 2 PQRs ;

·         PQR-1 Base Metal P355 GH Thickness : 8mm Process 1)Root : SMAW 2)Hot-Fill-Cap : SAW Back Weld: SAW 

·         PQR-2 Base Metal P355 GH Thickness : 8mm Process 1)Root : SMAW 2)Hot-Fill-Cap : SMAW Back Weld: SMAW  

 

My question is whether i can combine these 2 PQR for generating a new WPS ;                

·         Generated WPS : Base Metal Thickness : 16mm Process 1)Root : SMAW 2)Hot-Fill-Cap : SAW Back Weld: SMAW

 

Is it possible to use PQR-1 & PQR-2 for generating WPS for usage of SMAW for the back weld ?  What bothers me and makes me feel i should get advisory is since QW-200.4 (b) says;  For GTAW, SMAW, GMAW, PAW, and SAW, or combinations of these processes, a PQR for a process recording a test coupon that was at least 1/2 in. (13 mm) thick may be combined with one or more other PQRs recording another welding process and any greater base metal thickness.  Since my PQRs are carried out with 8mm thck. is it possible for me to combine them and apply SMAW Back Weld instead of SAW or not? 

Best Regards;

Demir

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACj12PCk4tK3uVEu5h4%2BAbqpA6Z7s8pSw0s7XfnjXv9FLOnG1Q%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.



--

Saygılarımla / Regards


Tuğrulhan ÖZDEMİR

API 653 AI, Welding & Materials Eng.

ASNT VT, PT, MT, RT L-II

+90 539 747 2676


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABSWRjoWNC5xA4j9tqPCrUkrgZD98xe6jOa%2BDVDr9K8agFFKiw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...