Hi!
Yes you can weld directly ss304L to Ss904 as it is a support and not coming in to contact of service atmosphere
Regards
Hegde
On Wednesday, 25 May 2016 9:17 AM, Makrand Sakpal <makrands9@gmail.com> wrote:
Dears,
We have one atmospheric hygienic (Food Industry) vertical vessel of SS904L material which is supported on legs. Vessel diameter is 3200 mm & TL-TL is 5100 mm.
The question is, can we weld SS304 directly on SS904L so that we can use SA-312 TP304 pipe l;eg supports?
Is it necessary to have SS904L RF pad instead of SS304?
Can there be an issue with weldability of SS904L with SS304?
Note : - We can't go for skirt support option.
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1a8c9b3e-1a20-4200-9d03-cba7a922c1ad%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
Comments