Thursday, March 19, 2015

Re: [MW:22985] Re: Tolerance for Dog leg

The relevnt tolerances have been illustrated in PFI ES3
 
Thanks,
Ash

On Tuesday, February 12, 2008 at 6:44:53 PM UTC+7, quality wrote:

It seems to be a process piping with design code ASME 31.3.

If the fabrication/ construction code is ASME B 31.3, it also permits a miter bend upto 3° is acceptable (ref ASME B 31.2 Article 304.2.3).

In other words, a deviation/ deflection upto 3° can be considered as straight pipe & does not effect the design conditions (unless otherwise this tolerance is over ruled by designers with a strict requirement for maintaining a slope or aesthetic appearance is important than the allowable tolerance). Then do not look further for acceptance tolerance. Rectify the joint & make it straight.

best regards,

Sanjeevan 

Gulf Petrochemical Services, Muscat, Oman 

 

----- Original Message -----
Sent: Tuesday, February 12, 2008 2:37 PM
Subject: [MW:565] Re: Tolerance for Dog leg

Here by attached the photo related to typical dog leg.
We are facing this problems in construction stage of plant piping. Allowing 3 Deg as tolerance appears to be more liberal and in lines like relief /blow down where slope of the line is  to be maintained process point of view. 
Thank you very much to all of you for your prompt reply.
 
Regards
 
Srs reddy
Saudi Aramco
 
 
 
 
 
On 2/11/08, Shyam Herur <herur...@gmail.com> wrote:
Can you specify the pipe spec and what it is used for ? Since you are referring to "line pipe" I presume its the pipe covered in spec API 5L. However I did find an abstract which  goes" usually out of straightness of pipe usually follows a log normal distribution with diametre, and, as would be expected the larger the diametre of the pipe, the straighter is the pipe. API 5L allows  24mm in a 12m joint. usually it is possible to obtain pipe to 12mm in 12m. to reduce total cost over specification of straightness should be avoided".
 
also refer to API 5L for further details.

 
On 2/11/08, Sankepalli R.S.Reddy <sankepall...@gmail.com> wrote:
It is the out of straightness of line pipe. The out of straightness may be due to weld distortion at joint locations or due to improper fitup.
regards

 
On 2/11/08, Raghuram Bathula <raghura...@gmail.com> wrote:

Can you please explain the term Dog leg, i have no idea what it is?
Is it a term related to steel structure? type of stair case
arrangement?

On Feb 11, 7:39 pm, "Sankepalli R.S.Reddy"
<sankepalli.rsre...@gmail.com> wrote:
> *Dog leg or out of alignment of line pipe:*
> **
> Can any body gives permissible tolerance for Dog leg. Whether any standard
> is covering this tolerance.
>
> Thanks and regards
>
> S. Rama subba reddy
>
> Inspection Engineer
>
> Khursaniya Gas Project, KSA
>
> Bldg 7, Cu 1
>
> Ph no: 6770120







No virus found in this incoming message.
Checked by AVG Free Edition.
Version: 7.5.516 / Virus Database: 269.20.2/1272 - Release Date: 11/02/2008 05:28 c

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/39e2e544-ea0b-4015-9d58-d49dfdc3dfed%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...