[MW:22988] FW: 22982] Welding Consumable selection

( P NO.1 G 2  ) to  ( P NO 1 G 2 or 1 " ASTM A 519 )

Use ER 70S-6 or -3 // 100% co2  // PWHT & preheat according to thickness "check ur construction code "

 

Ahmed Osman

Welding Eng.

ASNT NDT level III

API 510 inspector

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Siva Chidambaram
Sent: Tuesday, March 17, 2015 11:42 AM
To: materials-welding@googlegroups.com
Subject: [MW:22982] Welding Consumable selection

 

Hi experts,

 

I am going to weld a butt of Weld neck Flange to hammer union as per ASME Sec. IX.

 

Flange material: ASTM A 694 F60

Hammer union material: AISI 4130

Process: GMAW

 

Can anybody suggest, what welding consumable shall I use?

also suggest me the preheating and PWHT for the same.

 

Thanks and regards,

M. Sivachidambaram

QHSE Engineer

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPJQpMWFVQTb-3dpUmQjJ4NhHjK2oJz0scYop8Ef942i00qFLA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...