Thursday, March 5, 2015

[MW:22943] RE: 22938] EN 10204 3.1 certification

Vendor Quality Control can transfer the data and is authorized to certify in their own 3.1 certification.

Regards

 

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Sadique Sheikh
Sent: 05 March 2015 15:21
To: materials-welding@googlegroups.com
Subject: [MW:22938] EN 10204 3.1 certification

 

Dear All,

While during inspection of valves, pressure parts (body, bonnet, stud & nut) requirement were 3.1 certification as review point as per ITP for us Vendor certified the requirement on their letter head as 3.1 including chemical, mechanical & heat treatment requirement  with heat no. instead of providing MTC's of component manufacturer separately.

My question is, Shall we accept such MTC on valve manufacturing letter head instead of component manufacturing MTC?

Regards,

Mohd. Sadique Sheikh

 

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAH%2BBshCBeWV7OR3U3RgjeTLJqf1PqaUiJCsOQ%3DcZsfmMkQE7Vw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

 
 
!-- Virus-Free Mail Using AntiVirus for PostMaster Enterprise & QuickHeal Engine --!

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...