Sir,
which design code is used whether ASME 31.4 or ASME 31.8.
Sent from Samsung Mobile
-------- Original message --------
From: Amul Raj
Date:05/03/2015 11:58 (GMT+03:00)
To: materials-welding@googlegroups.com
Subject: [MW:22939] Requirements Of PWHT for the Cross Country Pipe Lines - Reg
Dear Experts,
-- We have done PQR with PWHT for the Material APL 5L Grade X60, and the coupon Size is 40 Inch & the Thickness is 38 mm with the Construction code application of API 1104 (Cross Country Pipe Line)
Based on the results we prepared WPS Also, But, As per API 1104 for 38.00 mm THK PWHT is not required
Now The Aramco PID instructed to follow the WPS to do all the Joints PWHT
What is the remdy for this & hat should we do
Kindly drop your advise
Thanks & Warm Regards,
Amul Raj T
QA/QC Welding
Samsung Engg, KSA
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/2f252b05-3866-481c-9fcf-2357a5f0c95e%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
Comments