Re: [MW:22951] Requirements Of PWHT for the Cross Country Pipe Lines - Reg

Refer scope of work,  Isometric drawing and P & ID to find the applicable code.
Section 434.8.9 specifies about PWHT is ANSI B 31.4

Regards,
Anup

On 6 Mar 2015 08:59, "'mv_srinivasan' via Materials & Welding" <materials-welding@googlegroups.com> wrote:
Sir,
which design code is used whether ASME 31.4  or ASME 31.8.


Sent from Samsung Mobile


-------- Original message --------
From: Amul Raj
Date:05/03/2015 11:58 (GMT+03:00)
To: materials-welding@googlegroups.com
Subject: [MW:22939] Requirements Of PWHT for the Cross Country Pipe Lines - Reg

Dear Experts,

We have done PQR with PWHT for the Material APL 5L Grade X60, and the coupon Size is 40 Inch & the Thickness is 38 mm with the Construction code application of API 1104 (Cross Country Pipe Line)

Based on the results we prepared WPS Also, But, As per API 1104 for 38.00 mm THK PWHT is not required 

Now The Aramco PID instructed to follow the WPS to do all the Joints PWHT

What is the remdy for this & hat should we do 

Kindly drop your advise 


Thanks & Warm Regards,

Amul Raj T

QA/QC Welding 

Samsung Engg, KSA  



 




--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/2f252b05-3866-481c-9fcf-2357a5f0c95e%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/bx0ck71s8shh6put0pe6ceia.1425578687428%40email.android.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJsQutYVhgDnOXS2Cx2NuqVxUEtdST1CA3465R6j_3tQOudMUQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...