Dear Mr. Prakash,
Thanks for your reply. Also regret for the language I used.
But i would like to get clarified a point that EN 10204 2.2 document content is "Statement of compliance with the order, with indication of results of nonspecific inspection"

I take the statement in this way.The \manufacturer will comply to the order requirement, but the results need not match with the items actually produced.(non- specific inspection). If it is non specific then why i need to match the qty with the batch lot. 
Thanks and regards
Vadivel. M

On Wednesday, March 4, 2015 at 10:05:12 PM UTC+5:30, Prakash Gotimukul wrote:
The certificate must match the requirement of a batch with Qty or any other means to correlate. It cannot be any certificate unrelated to the actual product/s.
By the way we dont like to throw at you. We will politely give you. ( pun intended)

Rgds
G.Prakash
AIS, AIA LLC TX, USA
Technical Director, Hitek Engg Services, Dubai
 gpraka...@gmail.com.
Tel: +9714 2778511 Mob:+97152 979 5678

On Wed, Mar 4, 2015 at 1:22 PM, Vadivel Mahadevan <vadivel...@gmail.com> wrote:
Dear Experts,

Can you please throw me an Idea whether we need to match the Quantity for EN10204 2,2 Certificates. 
Supposedly consider a lot of around 30 nos of a pressure part where customer has requested for EN 10204 2.2 Certification for internals. Whether I am supposed to submit him internals Test certificate to match this 30 nos or a sample TC is sufficient enough.

What is the procedure to raise this issue to EN body?

Thanks and regards
Vadivel. M

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1631183a-cb20-4d72-82bc-197dd5948d32%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/af9f5342-03f8-490d-be43-a8d904ad1399%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...