Monday, March 16, 2015

Re: [MW:22977] Normalized plate of A516 gr 70

As per my point of view ,above stated 1&2 criteria acceptable then u can proceed.  

On Sat, Mar 14, 2015 at 7:14 PM, Dani Darwis <daniyd@centrin.net.id> wrote:

Dear Expert,

 

Our vendor had purchased normalized plates from Sumitomo of steel making and Mill Cert clearly stated that the plates have been normalized but no sign or stamp "N" on plate. The problem is when the client reviewed and witnessed it, they don't believe that the plate has been normalized and the question is what test needs to be conducted to prove that the plate has been normalized?

 

For your info: what do you think if the client ask for the following test:

1.       Tensile test and the specimen needs to be normalized first prior to test, acceptance criteria as per mill cert.

2.       Scanning Electron Microscope (SEM), acceptance criteria: no residual stress in the plate.

 

Your quick response is highly appreciated.

 

Regards

Dani

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/003101d05e5d%240d0168b0%2427043a10%24%40net.id.
For more options, visit https://groups.google.com/d/optout.



--
G.Gopalakrishnan
Welding Engineer
Mukand Ltd
Mumbai
Moble :+91-9833397917

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOp_kKjMkjLbLMW9AKZBugrP8vsZYhEoW6Sedu_v5acFAytTzQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...