Hello Raj,
 
While Working on any project, you need to consider the client specification and the reference Code/Standard as stipulated in the contract document. Where there is conflit, the most strigent condition supercedes or issue a technical query to your client for clarification.
 
As per your query, you will need to check your client specification, they may have specifiy that PWHT is performed on such thinckness as 38mm and beside, your qualify WPS shall be limited to PWHT requirement and cannot be used otherwise.
 
I have a question for you, why did you qualify the WPS with PWHT if you do not want to use it and if you know the requirement of API 1104. What was on your mind when you are performing the WPQR and to what code have you qualified it?
 
Regards,
 
Rems Okonkwo (IWE)
On Thu, Mar 5, 2015 at 9:58 AM, Amul Raj <win.amul@gmail.com> wrote:
Dear Experts,

We have done PQR with PWHT for the Material APL 5L Grade X60, and the coupon Size is 40 Inch & the Thickness is 38 mm with the Construction code application of API 1104 (Cross Country Pipe Line)

Based on the results we prepared WPS Also, But, As per API 1104 for 38.00 mm THK PWHT is not required 

Now The Aramco PID instructed to follow the WPS to do all the Joints PWHT

What is the remdy for this & hat should we do 

Kindly drop your advise 


Thanks & Warm Regards,

Amul Raj T

QA/QC Welding 

Samsung Engg, KSA  



 




--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/2f252b05-3866-481c-9fcf-2357a5f0c95e%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEpWm6ub2NfeJ6eMEqikBtkNPokiA%2BhYVkViKxPpTT81j7rb2w%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...