[MW:20099] Re: WATER TESTS

Dear sampath prior to start Hydro test following water test should be done;
1) Method of sampling and test(physical and chemical) for water and wast water( PH value, Acidity, Alkalinity, Dissolve oxygen) as per IS-3025.
2) & 3)To Prevention of metal corrosion.
Strictly follow the API Standard(11th or latest) as article 7.3.6 for Hydrostatic testing requirements.
Thanks
P.kumar
    

On Thursday, February 13, 2014 6:43:16 PM UTC+5:30, Sampath Kumar wrote:
Dear Experts,

We are in the process of doing Hydro test for a storage tank.The tank will be filled with water which is being stored since  more than 2 months in a waste water pump in open atmosphere.MY question is[1] what are all the necessary important test to be carried for that water.[2] why those test to be done[3]What will happen if we use that water for the test. pls give your expert opinion with code reference.
Thanks & Regards
Sampath


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...