Friday, February 28, 2014

Re: [MW:20196] Mutiple WPS from single PQR

no / because the recording process as GTAW less than 13mm .

Sent from Yahoo Mail on Android



From: mahammed javeed <javeedcwi@gmail.com>;
To: <materials-welding@googlegroups.com>;
Subject: [MW:20190] Mutiple WPS from single PQR
Sent: Thu, Feb 27, 2014 11:58:40 AM

Gents,

I have PQR with impact test requirements and the details are below like this.

Base material thickness 11mm with impact test requirements
Process GTAW & SMAW

base metail qualified range 11mm- 22mm

GTAW process deposited weld metal qualified range 8 mm
SMAW process deposited weld metal qualified range 14mm

Now I want to make a WPS for a job of 6mm only using GTAW process, I have found a difficulty in understanding the base metal thickness range qualified. 

Can I consider only weld metal deposited thickness range this process and make a WPS?

Regards
M. Javeed


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

[MW:35738] ASME IX WPS Qualification Query: GTAW + FCAW with Multiple PQRs

Dear Welding Experts, I'm currently preparing a Welding Procedure Specification (WPS) and have encountered a request to qualify a GTAW +...