[MW:20111] Reduction in % ferrite of UNS S31803 weld after Post forming HT

Dear Experts,

In one of our project, one coil pipe to pipe butt weld was undergone PWHT @ 1080º C. for 12 minutes soaking period and rapid water quenching after forming a pipe in coil form. Pipe size is 21.3 mm. O.D. X 2.77 mm. W.T. SA 790 UNS S31803. We have used ER 2209 filler wire with GTAW process. 

After solution annealing, % ferrite was measured 8-10 using fisher make calibrated ferritescope instead of required 30-60%. PQR was established in the same pipe size and material Grade. In PQR, after PWHT @ 1020º C. for 10 minutes and rapid water quenching, % ferrite was coming average 38 in point counting method as per ASTM E 562.

What shall be the reason of reduction in % ferrite in production weld? What shall be the corrective action to achieve % ferrite between 30-65%. In this forum, some where I have read that heating to temperatures approaching 1100º C will dissolve some or all of the ferrite, depending on the hold time at temperature, composition of the weld metals, and the as-welded ferrite content. I need some reference book on this issue.

Thanks & regards,

C. R. Gandhi

      

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...