I hv'nt seen such requirement or restriction.
any way as part of good workmanship maximum 2 times is suitable to maintain HAZ property or else cut up to HAZ each side to facilitate new HAZ.
Fitting joints more times CRW very difficult,especially elbow,TEE.
Number of cut and re weld depend whether it is SS or CS materials.
For SS,DSS,SDSS special care should be taken avoid re repair to control ferrite number,corrosion property.
Hope this help.
Regards
Mohd.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
any way as part of good workmanship maximum 2 times is suitable to maintain HAZ property or else cut up to HAZ each side to facilitate new HAZ.
Fitting joints more times CRW very difficult,especially elbow,TEE.
Number of cut and re weld depend whether it is SS or CS materials.
For SS,DSS,SDSS special care should be taken avoid re repair to control ferrite number,corrosion property.
Hope this help.
Regards
Mohd.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
Comments