Since it wasn't in service and under sea for a year only, there are no special tests to my belief.

All one does is to carry standard checks that are done on pipes. May be you can check pipe thicknesses at random, weld quality and chemical check on surface for comparing with previous results esp. to indicate sea erosion/ corrosion.

If you are planning to re use, it can be done with mutual consent and set procedure for acceptance.

Best Regards,

Vinod Bhatt


On Mon, Feb 17, 2014 at 11:57 AM, vinod kumar <vinodmylaraiah@gmail.com> wrote:
Dear peers,
what are the tests we can conduct on retreived sub sea pipe line from sea to check the pipe integrity.
Pipes were in sea for more than a year and pipe grade is API 5L X 60 Grade.
It was not under service condtion.
If you have any procedure please share with me.
--
Thanks and Best regards

M. Vinod Kumar

"Never Explain yourself to any one Because the person who likes you doesn`t need it, and the person who dislikes you won`t believe it."

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

[MW:35614] Re: SS FILLER

dear , pl check A number and Gas composition use for ss cant be sutibale same % for duplex., u need to qualified with aditional testing of f...